Add to Cart
LT07 Permanent Hard Ferrite Magnets -80~150℃ Working Temperature
Quick Details:
1. Application: Automotive seating motor
2. Material grade: LT02,LT04, LT07
3. Shapes: arc, segments, alien
4. Type: permanent ferrite magnet, wet-pressure magnet,sintered ferrite magnet
5. Material: ferrite, strontium, La2O3, CoO
Permanent ferrite magnet is one of the most cost effective magnetic materials. Composed of Barium or Strontium ferrite, these materials exhibit good resistance to demagnetiztion, and are the lowest cost materials available today. It has a fair to good resistance toward corrosion and it can operate in moderate heat. Ceramic magnet has low energy product and they are usually used in assemblies containing mild steel. Sintered ferrite magnets are hard and brittle and are extensively used in automotive, home appliances, industry controls, etc.
Applications:
DC motor
Permanent ferrite magnet DC motor
Speaker
Magnetron
Magnetor
Passive magnetic energy
Magnetic Door Catcher
Toys
Arts and Crafts
Advertisement
Training aid
Magunion Advantages:
Stable quality, good uniformity of performance and size.
School-enterprise cooperation, provide professional customized motor magnet program.
Professional new production line, the delivery time of sample is on 7-10 days.
Merchandise name:
Hard ferrite magnet, sintered magnet, powerful magnet, pot magnet, segment magnet, DC motor magnet, generator magnet, cylinder magnet, magnet material, magnetic product, permanent magnetic materials.
Physical Characteristics | ||||||||
Physical Properties | LT04 | LT05 | LT06 | LT07 | LT08 | LT09 | LT10 | LT11 |
Temperature Range (℃) |
-40~+80 | -40~+80 | -40~+80 | -40~+80 | -40~+80 | -40~+80 | -40~+80 | -40~+80 |
Electrical Resistivity (Ω·m) |
104~108 | 104~108 | 104~108 | 104~108 | 104~108 | 104~108 | 104~108 | 104~108 |
Density (g/cm3) |
4.8~5.0 | 4.8~5.0 | 4.8~5.0 | 4.8~5.1 | 4.8~5.1 | 4.7~5.0 | 4.8~5.1 | 4.7~5.0 |
Recoil Permeability(rec) | 1.05~1.03 | 1.05~1.03 | 1.05~1.03 | 1.05~1.03 | 1.05~1.03 | 1.05~1.03 | 1.05~1.03 | 1.05~1.03 |
Curie Temperature θt(℃) |
460 | 460 | 460 | 450~460 | 450~460 | 450~460 | 450~460 | 450~460 |
Temperature Coefficient of Remanence Br(%℃) | -(0.18~0.2) | -(0.18~0.2) | -(0.18~0.2) | -(0.18~0.2) | -(0.18~0.2) | -(0.18~0.2) | -(0.18~0.2) | -(0.18~0.2) |
Linear Expansion Coefficient(10-6/℃) | 9~15 | 9~15 | 9~15 | 9~15 | 9~15 | 9~15 | 9~15 | 9~15 |
Magnet Properties | |||||||||
Type (Magunion) |
Type (TDK) |
Properties | |||||||
Br | Hcb | Hcj | BH(max) | ||||||
Gs | mT | Oe | kA/M | Oe | kA/M | MGOe | kJ/m3 | ||
LT01 | / | 3850±100 | 385±10 | >3100 | >246.8 | >3300 | >262.7 | 3.7±0.2 | 29.5±1.6 |
LT02 | FB5B | 4100±100 | 410±10 | 3200±150 | 242.4±11.9 | 3500±150 | 278.6±11.9 | 4.0±0.2 | 31.8±1.6 |
LT03 | / | 3950±100 | 395±10 | 3650±150 | 290.6±11.9 | 3900±150 | 310.5±11.9 | 3.8±0.2 | 30.2±1.6 |
LT04 | FB6B | 4200±100 | 420±10 | 3800±150 | 302.5±11.9 | 4000±150 | 318.4±11.9 | 4.2±0.2 | 33.5±1.6 |
LT05 | FB6H | 4000±100 | 400±10 | 3800±150 | 302.4±11.9 | 4500±150 | 358.1±11.9 | 3.7±0.2 | 29.4±1.6 |
LT06 | FB9B | 4500±100 | 450±10 | 4300±150 | 342.2±11.9 | 4500±250 | 358.2±11.9 | 4.9±0.2 | 38.4±1.6 |
LT07 | FBIH | 4300±100 | 430±10 | 4150±150 | 330.2±11.9 | 4800±250 | 382.1±11.9 | 4.4±0.2 | 35.0±1.6 |
LT08 | FB12H | 4600±100 | 460±10 | 4300±150 | 342±11.9 | 5000±250 | 398.1±11.9 | 5.2±0.2 | 41.4±1.6 |
LT09 | FB12B | 4700±100 | 470±10 | 4250±150 | 338.4±11.9 | 4700±250 | 374.2±11.9 | 5.4±0.2 | 43.1±1.6 |
LT10 | FB9N | 4600±100 | 460±10 | 3500±150 | 278.5±11.9 | 3600±150 | 286.5±11.9 | 5.1±0.2 | 40.4±1.6 |
LT11 | FB6N | 4400±100 | 440±10 | 3250±150 | 258.6±11.9 | 3300±150 | 262.7±11.9 | 4.5±0.2 | 35.9±1.6 |