LT08 Permanent Ferrite Magnet , Hard Ferrite Magnet for Automotive Window Adjusting Motor
Quick Details:
1. Application: Automotive window adjusting motor
2. Material grade: LT05,LT07, LT08
3. Shapes: arc, segments
4. Type: hard ferrite magnet, sintered ferrite magnet
5. Material: ferrite, strontium, La2O3, CoO
Barium ferrite (BaO.6Fe2O3) and Strontium ferrite (SrO.6Fe2O3) are mainly two types of ferrite magnets. Compared with other permanent magnets, sintered ferrite magnet is cheap. It is suitable for most sensitive, but need not very high performance applicatoins. As a non-metal magnets, it is an ideal product for applications that require non-rusty magnets in humus environment. Sintered ferrite magnets are widely used in many different applications, such as automotive, home appliances, loudspeakers, and many special applications.
Applications:
DC motor
Hard ferrite DC motor
Speaker
Magnetron
Magnetor
Passive magnetic energy
Instrument and Meters
Toys
Arts and Crafts
Magunion Advantages:
Stable quality, good uniformity of performance and size
School-enterprise cooperation, provide professional customized motor magnet program.
Professional new production line, the delivery time of sample is on 7-10 days.
Merchandise name:
Permanent magnet, wet-pressure magnet, sintered magnet, arc magnet, DC motor magnet, generator magnet, cylinder magnet, magnet material, magnetic product, permanent magnetic materials.
Physical Characteristics | ||||||||
Physical Properties | LT04 | LT05 | LT06 | LT07 | LT08 | LT09 | LT10 | LT11 |
Temperature Range (℃) | -40~+80 | -40~+80 | -40~+80 | -40~+80 | -40~+80 | -40~+80 | -40~+80 | -40~+80 |
Electrical Resistivity (Ω·m) | 104~108 | 104~108 | 104~108 | 104~108 | 104~108 | 104~108 | 104~108 | 104~108 |
Density (g/cm3) | 4.8~5.0 | 4.8~5.0 | 4.8~5.0 | 4.8~5.1 | 4.8~5.1 | 4.7~5.0 | 4.8~5.1 | 4.7~5.0 |
Recoil Permeability(rec) | 1.05~1.03 | 1.05~1.03 | 1.05~1.03 | 1.05~1.03 | 1.05~1.03 | 1.05~1.03 | 1.05~1.03 | 1.05~1.03 |
Curie Temperature θt(℃) | 460 | 460 | 460 | 450~460 | 450~460 | 450~460 | 450~460 | 450~460 |
Temperature Coefficient of Remanence Br(%℃) | -(0.18~0.2) | -(0.18~0.2) | -(0.18~0.2) | -(0.18~0.2) | -(0.18~0.2) | -(0.18~0.2) | -(0.18~0.2) | -(0.18~0.2) |
Linear Expansion Coefficient(10-6/℃) | 9~15 | 9~15 | 9~15 | 9~15 | 9~15 | 9~15 | 9~15 | 9~15 |
Magnet Properties | |||||||||
Type (Magunion) | Type (TDK) | Properties | |||||||
Br | Hcb | Hcj | BH(max) | ||||||
Gs | mT | Oe | kA/M | Oe | kA/M | MGOe | kJ/m3 | ||
LT01 | / | 3850±100 | 385±10 | >3100 | >246.8 | >3300 | >262.7 | 3.7±0.2 | 29.5±1.6 |
LT02 | FB5B | 4100±100 | 410±10 | 3200±150 | 242.4±11.9 | 3500±150 | 278.6±11.9 | 4.0±0.2 | 31.8±1.6 |
LT03 | / | 3950±100 | 395±10 | 3650±150 | 290.6±11.9 | 3900±150 | 310.5±11.9 | 3.8±0.2 | 30.2±1.6 |
LT04 | FB6B | 4200±100 | 420±10 | 3800±150 | 302.5±11.9 | 4000±150 | 318.4±11.9 | 4.2±0.2 | 33.5±1.6 |
LT05 | FB6H | 4000±100 | 400±10 | 3800±150 | 302.4±11.9 | 4500±150 | 358.1±11.9 | 3.7±0.2 | 29.4±1.6 |
LT06 | FB9B | 4500±100 | 450±10 | 4300±150 | 342.2±11.9 | 4500±250 | 358.2±11.9 | 4.9±0.2 | 38.4±1.6 |
LT07 | FBIH | 4300±100 | 430±10 | 4150±150 | 330.2±11.9 | 4800±250 | 382.1±11.9 | 4.4±0.2 | 35.0±1.6 |
LT08 | FB12H | 4600±100 | 460±10 | 4300±150 | 342±11.9 | 5000±250 | 398.1±11.9 | 5.2±0.2 | 41.4±1.6 |
LT09 | FB12B | 4700±100 | 470±10 | 4250±150 | 338.4±11.9 | 4700±250 | 374.2±11.9 | 5.4±0.2 | 43.1±1.6 |
LT10 | FB9N | 4600±100 | 460±10 | 3500±150 | 278.5±11.9 | 3600±150 | 286.5±11.9 | 5.1±0.2 | 40.4±1.6 |
LT11 | FB6N | 4400±100 | 440±10 | 3250±150 | 258.6±11.9 | 3300±150 | 262.7±11.9 | 4.5±0.2 | 35.9±1.6 |